NO NITRIC ACID CELL PHONE GOLD PLATED CONNECTORS GOLD RECOVERY | GOLD RECOVERY WITHOUT NITRIC ACID
Gold recovery NO nitric acid from old cell phone connectors, watch this video and GIVES ME thumps up.. thanks for Watching.
Gold recovery NO nitric acid from old cell phone connectors, watch this video and GIVES ME thumps up.. thanks for Watching.
Пікірлер: 108
Salamut Po Cabayan. My Tagalog is not so good. However I worked in a gold refinery and there is one modification you can make so you never loose your gold. Take the gold in your filter paper and put it in a crucible and heat from the bottom with a flame. This will burn up the paper and will make the gold powder stick together. Then later you can it it with a torch to melt it.
@PoorMiners321
Жыл бұрын
oo salamat sa magandang idiya kabayan God bless you..
wow nice process very effective result thanks for sharing bro..
@PoorMiners321
Жыл бұрын
your welcome bro
Salamat boss sa sharing
@PoorMiners321
Жыл бұрын
Welcome boss
Great job! That's a nice 1 g of candy ;-)
@PoorMiners321
Жыл бұрын
🤣🤣🤣 Thank you, I loss some of my gold during melting..
Good job bro! 💥🔥👍
@PoorMiners321
9 ай бұрын
Thank you too bro..
Congratulations
@PoorMiners321
Жыл бұрын
Thank you❤
Thanks 🙏
@PoorMiners321
Жыл бұрын
You’re welcome 😊
Emeğinize sağlık çok güzel çalışma olmuş👍👍.Ustam bende bakır solüsyonu var,evde yapıyorum sizinki kadar imkanım yok evdeki malzemelerden ne ile çöktürebilirim.Bir sorum daha var ısıtmada kullandığınız tavanın içindeki malzeme alüminyummu beher ile tavanın arasındaki ince malzemeyi sordum.Şimdiden teşekkürler.
@PoorMiners321
Жыл бұрын
Thank you, your copper solution you can use it to extract gold plated feom mobile phone, you can precipitate gold using iron sulfate but most prepare is sodium metabi sulfite is better.
@PoorMiners321
Жыл бұрын
i use steel plate, dont use aluminun for heating.
@angelooldman7201
Жыл бұрын
@@PoorMiners321 why steel plate ,would you be so kind to explain this to me ? thank you budd have a great day
@salihakdag6371
Жыл бұрын
@@PoorMiners321 teşekkürler ustam ❤️👍
@PoorMiners321
Жыл бұрын
the one I put on the beaker, then i add pcb insolator on the top of steel plate to control heat from charcoal budd
Does it work with 30-31 % HCL to boiling or do i need 35% HCL , and nice video brother
@PoorMiners321
11 ай бұрын
Thanks brother, Yeah its working, sometimes very common concentrations 29% is working will also brother
Your awesome bro
@PoorMiners321
Жыл бұрын
Thanks bro❤
Hcl and hydrogen peroxide gold desolve riali???
@PoorMiners321
11 ай бұрын
Yes only gold plated are quicker to dissolved
Это наш шоколад))
Hi, would you be able to tell me if the sale of hno3 (nitric acid) is prohibited in the United States
@PoorMiners321
Жыл бұрын
maybe prohibited,the others have bought but the price is high, maybe just trick them
@enricotrombini9952
Жыл бұрын
No it is not.. Expensive tough.
Good
@PoorMiners321
Жыл бұрын
Thank you..
Love you❤❤❤
@PoorMiners321
Жыл бұрын
Thanks
Al parecer tambien hay plata, como precipitas la plata en solucion AP.
@PoorMiners321
4 ай бұрын
Yeah but silver are precipitate without doing anything because of hcl
Is there a vid with no nitric, cloro, hydro whatever, like at home basic in a apt with no ventilation method?
@PoorMiners321
16 күн бұрын
I'm sorry brother, there's no other way, all procedure involve mild acid, or maybe strong acid.
@1fnklown
14 күн бұрын
Good to know-thanks
Boss ano po ba ang dapat ilagay na acido para mabilis ericover ang mga plated gold salamat
@PoorMiners321
Жыл бұрын
tubig lang yan boss, at nitric acid, halimbawa, yung scrap mo lailangan matakpan ng tubig, na distilled water hindi yung top water sa grepo kasi may chlorin yung sa grepo,tapos measure mo lang ang þubig kung ilang ML yun, pero dipindi yan sa scrap halimbawa gold plated pins, kailangan 1 is to 1 ration kung natakpan ang scrap gold plated pins sa distilled water ng 300ml, ganun din ang nitric acid, kung scrap gold plated finger gaya ng ram stickpwedi yan sa 1 to 2 ratio halimbawa natakpan ang scrap sa 400ml distileed water 200ml din ang nitric yan ang madali hindi kumplikado ang trabaho napaka dali matanggal ang gold doon.
Whate carat of this gold?
@PoorMiners321
Жыл бұрын
maybe not less than 18k
how many milimeters is your fabric filter or paper ?
@PoorMiners321
Жыл бұрын
30mm filter paper, around 400ml
@ahmettezcan-xi3gm
Жыл бұрын
@@PoorMiners321 thank you so much
@PoorMiners321
Жыл бұрын
👍
Sir, how did it come together as you said, what should I do next?
@PoorMiners321
Жыл бұрын
sorry i don't understand what you mean. please be a little clear my friend
@SRI98822
Жыл бұрын
Sir come to fb messenger sir
@SRI98822
Жыл бұрын
Sir
@PoorMiners321
Жыл бұрын
ok go to Poor miners page
Boss pag pinakuluan walang muriatic na i dadagdag sa tubig.o mayron pa
@PoorMiners321
27 күн бұрын
Sa paghuhugas ba ibig mong sabihin? Kung sa paghuhugas na e wala ng muriatic yun
@user-fl9ih9dy9y
27 күн бұрын
@@PoorMiners321 diba pagkatapos mo tanggalan ng maraming tubig pinakuluan mo naman sa tubig peru diko nakita sa vidio na nilagyan mo ng muriatic pero sa ibang vlog mo nilagyan mo ng muriatic at tubig bago mo pakuluan salamat
@PoorMiners321
27 күн бұрын
Oo yan kasi ang tamang paraan, kasi ang sabi ko doon, sundin nyo lang ang video tungkol sa washing na ginawa ko bro
good job bro. where you living ?
@PoorMiners321
10 ай бұрын
Thanks bro im from philippines
@malyshenkovolodymyr6785
10 ай бұрын
have alot of gold painting stuff for affinage
@malyshenkovolodymyr6785
10 ай бұрын
can send you big box in Philippines
@PoorMiners321
10 ай бұрын
Yeah but the shipment maybe too expensive .
Hello, I like your videos, I am your subscriber. Can you help me and advise me how to separate gold and sand from each other using chemicals?
@oo_oo1077
Жыл бұрын
I use nitric acid and hydrochloric acid to dissolve it but I can't neutralize the nitric acid. I tried I had no luck with urea, then iron sulphide has no results, I use hydrazine hydrot to recover.
@oo_oo1077
Жыл бұрын
Please do not leave my comment unanswered. Help me who has a similar problem
@PoorMiners321
Жыл бұрын
yeah, thanks by the about separation of two gold and sand we have two process is easy by using cyanide or smelting..
@oo_oo1077
Жыл бұрын
@@PoorMiners321 Thanks for the answer, but I can't get cyanide, it's punishable by law in my country. Can you give me your email or contact me and I'll send you photos of the process, maybe you can figure something out and help me.
@PoorMiners321
Жыл бұрын
Is not working because of sulfur, you need to roasting to remove sulfur first..and the best way are smelting process,
Boss kailan pala dagdagan ng sulfuric acid pag natunaw na yung gold foil...puwedi ba yung tubig ng baterry ang idagdag
@PoorMiners321
Ай бұрын
Oo pag natunaw na, 10% lang man yung sulfuric na galing sa battery, kung walang sulfuric optional man lang yun pwedi naman wala bro..
@user-fl9ih9dy9y
Ай бұрын
@@PoorMiners321 ah boss segi subukan ko yan ang dami kung naipon ngayun na gold foil.mga nasa 50 grams.na
@PoorMiners321
Ай бұрын
@user-fl9ih9dy9y ang sulfuric kasi bro, pang precipitate man langvyun sa lead, pero kung gold foil ang tunawin mo wala ng lead yun kasi para saakin di na kailangan yun, ang dami, siguradohin mo yan,
@user-fl9ih9dy9y
27 күн бұрын
Boss yung tinunaw ko na gold foil sa muriatic at hydrogen peroxide.pagkatapos nilagyan ko ng sodium metabulsulfite hindi bumaba ang sodium parang naging kulay brown yung tubig peru walang nalaglag sa ilalim na gold powder ano ang gagawin ko ditu boss dadagdagan kopa ulit ng sodium metabulsulfite patulong ako boss sayang yung pinagpaguran ko
Boss napakarami ko napong scrap na plated gold from cp. Kulng lng po Ako sa gamit baka po matulungan nyo po ako
@PoorMiners321
10 ай бұрын
Maganda yan boos, ano pung klasing tulong naiambag ko sa inyo?
Hello sir
@PoorMiners321
Жыл бұрын
yes
Idol anung dahilan bakit d na dedelute ung SMB sa hcl and bleach solution d nag pe precitate ung gold pls answer idol.
@PoorMiners321
Жыл бұрын
low acidity bro, kailangan mo dagdagan ng hcl at e heat mo ulit solution para tomaas yung acidity para mag react yung hcl sa smb at makapag create ng sulfur
@francisflores7486
Жыл бұрын
idol Papaanu gagawin sa d natunaw n smb kaylangan ko pa ba un i filter?
@PoorMiners321
Жыл бұрын
bakit hindi natitunaw? baka piki yung smb mo or expired
@PoorMiners321
Жыл бұрын
kunin mo nalang e filter mo cya
@francisflores7486
Жыл бұрын
Bro anu kya iba paraan para makuha ko ung gold sa solution konti lang naman un na curious lang ako sa kakapanood ko sayu at nakakahinayang din kasi kung d ko un makuha.
good morning budd, does this method work with none magnetic pins also?
@PoorMiners321
Жыл бұрын
good evening here budd, this process isn't work with non magnetic, because non magnetic is mostly copper and not easily dissolve with hydrochloric alone, but you can do that by adding small amount of hydrogen peroxide, in Acid peroxid method but do not heat your solution gold well dissolve.
@angelooldman7201
Жыл бұрын
@@PoorMiners321 thank you so much love your videos
@PoorMiners321
Жыл бұрын
Your welcome budd..
Your crucible broke because it does not look like you first seasoned it wirh borax it looks new. Always treat new crucible with borax before use.
@PoorMiners321
10 ай бұрын
Yeah that is our old crucible, i have new order but doesn't reveived yet and I cant wait because we need to upload video..
If you mix your SMB with water first there is less loss of SO2 gas during addition and you will use less SMB. Also ferrous sulphate is another way to precipitate gold and leaves all impurities in solution as it will drop only gold.
@PoorMiners321
Жыл бұрын
very good idea🤣
Love you❤❤❤
@PoorMiners321
Жыл бұрын
Thanks brother..