6G Welding Test | TIG Fill and Cap Pass | Full TIG Welding Procedure ! Part 2/2
Ғылым және технология
6G welding test with tig fill and cap pass on a 3" XXH wall, with a full tig welding procedure.
6G is where the pipe is fixed at a 45-degree angle and welded in this fixed position.
So, it basically covers flat, horizontal, vertical welding, and overhead in a single position.
In this video, I will break down the steps to pass the 6G position test, starting with the root pass, and in the second video, I will show the steps from fill passes to finish with a multi-pass cap.
The pipe welding techniques used, and the welding procedure is also identical to the AWS D1.1 and ASME Section IX welder performance qualification (WPQ) pipe welding certification. As per ASME Section IX.
#tig #tigwelding #6G
All of my videos are recorded at working sites in various locations and different welding positions.
90% of my welding projects in videos are x-rayed, and if you like to see hands-on projects, welcome!
If you liked this video please give it a thumbs up, share it, subscribe and click the bell.
It doesn’t cost you anything but massively helps my KZread channel. Thank you.
Support this channel with 🔔 Subscribe and 👍 Like!
/ x3mtig
Пікірлер: 37
Excellent video brother! Thanks for unselfishly sharing your knowledge with us! 👍🏾
@X3MTIG
Жыл бұрын
Thanks brother 👍
Man you are one hell of a welder. Your information is right to the point. Thank you for taking the time to make these videos. They are excellent . I'm also one of you first subscribers. Again love the channel
@X3MTIG
2 жыл бұрын
Thank you very much for your comment brother, and for your support .🍻💪
@user-ft7jy1hf1p
Жыл бұрын
Х8
Amazing video brother! 😊 👍🏻
@X3MTIG
2 жыл бұрын
Thanks brother 👍
Thank you for these I work in the that shop so helpful
@X3MTIG
2 жыл бұрын
Thanks bud
What was your amperage on the cap? Did you let the pipe cool before the cap? I always undercut that last bead. Can’t seem to get away from it.
Muy buen video saludos desde Argentina
@X3MTIG
2 жыл бұрын
Thank you my friend, greetings to beautiful Argentina 🇦🇷
Nice👏👏👏👏
Good job hero
nice , I am a thousand subscriber:)
@X3MTIG
2 жыл бұрын
Haha 😆 yes you are, and thank you for that 🙏 Definitely you will be remembered for that 🍻👍 soon as I got some merchandise it will go to your address. Thanks for your comment and support!
Nice❤
Greet job
Excellent video so when u start to fill the sides u start at top first and stack down? Is this the same in the 2g position? Thanks bro
@X3MTIG
2 жыл бұрын
Hey bud thanks for the comment. It all depends from the fit up and how it turns out after the root pass, but generally I always go from the bottom part and do fill passes to the top part, that’s for 6G. In 2G position after the root pass I generally start at the top part first, bottom, and run one through the middle.
Gotta test booked in for next week,What is your gas pressure setting on? Also did you use a grinder to blend in your start stops at all?cheers great video
@X3MTIG
2 жыл бұрын
Thanks for your comment bud. Gas pressure is at 15 lpm , and yes I was allowed to use grinder .
@curlybizkit5384
2 жыл бұрын
@@X3MTIG every start/stop you blended in from root/fill and cap?
@X3MTIG
2 жыл бұрын
@@curlybizkit5384 only for the root part.
@curlybizkit5384
2 жыл бұрын
@@X3MTIG passed my test!!! Thanks X3M Tig!!!
@X3MTIG
2 жыл бұрын
@@curlybizkit5384 that’s a great news brother 💪
Best ❤️
@X3MTIG
2 жыл бұрын
Thank you my friend!
How much amps caping
what size tungsten?
@X3MTIG
Жыл бұрын
1/8
We had a van pull up to a facility and try to jab everyone in the plant the other week. I stayed inside the boiler and ate a peanut butter and jelly and pissed in a couple water bottles till the end of the day. I swear they want you to become a 5g antenna 📡 for the devil 🤘. I ain't doing that shit. Very nice weld BTW
I hate background music 🎶...
REALLY?, HAGOJIBI THEME MUSIC?... SHAMELESS!.. LOL
@X3MTIG
Жыл бұрын
Ohh, I didn’t know he’s musician and got his own music! The last time I checked he was a welder and like everyone else on KZread using free music library! 🙄🤦🏻♂️
Very nice this video excellent#khanbiharguru
@X3MTIG
2 жыл бұрын
Thanks buddy 👍