Guide to metal finishing techniques, heat shrink in detail, to a file finish.

Автокөліктер мен көлік құралдары

Comprehensive guide to the art of metal finishing with Peter from Mobile Car Restoration. In this video, we cover traditional skills and techniques that are the cornerstone of metal finishing, also called file finish. This is a must-watch for automotive restoration enthusiasts eager to learn and master new skills. Today, we are focusing on the process of metal finishing a Porsche 356 roof.
Metal finishing is a time-honored craft that involves shaping and smoothing metal to achieve a flawless surface. Unlike modern methods that rely heavily on body fillers, traditional metal finishing uses tools and techniques to remove imperfections and restore the metal to its original form. This video aims to provide you with a solid foundation in these methods, ensuring you have the skills to tackle your own restoration projects.
Our video provides a detailed walkthrough of the metal finishing process on a Porsche 356 roof, from start to finish. We start by evaluating the condition of the Porsche 356 roof. Identifying dents, warps, and stretched areas is crucial for planning the work ahead.
Using hammers and dollies, we demonstrate how to gently coax the metal back into shape. This involves a series of careful taps, working the metal in small increments to avoid overworking and causing further damage.
For areas where the metal has stretched, heat shrinking is essential. We show you how to use a torch and shrinking disc to carefully heat the metal, causing it to contract and regain its original form. This step requires precision and patience, and we provide tips to avoid common pitfalls.
Once the major imperfections are addressed, we use flippers to further smooth the surface. This step helps distribute the metal evenly and prepares it for the final finishing touches.
The final step involves using files to remove any remaining high spots and create a perfectly smooth surface. This step is crucial for achieving a professional look and ensuring the metal is ready for primer and paint.
Throughout the video, we share insider tips and tricks to make the process easier and more effective:
Patience is Key: Metal finishing is an art that requires time and precision. Rushing the process can lead to mistakes and subpar results.
At Melomotive, we are passionate about sharing our knowledge and expertise with fellow automotive enthusiasts. Our team has high-level experience with techniques and materials in automotive refinish and best practices for restoration. Whether you're working in a home workshop or running a professional garage, our videos are designed to help you achieve the best results in your projects.

Пікірлер: 35

  • @daos3300
    @daos330019 күн бұрын

    what a great vid. started a little long winded but really gets into the hands-on detail by the end. if this series continues i'll definitely be subscribing.

  • @melomotive14

    @melomotive14

    10 күн бұрын

    Thanks

  • @waynelea3468
    @waynelea3468Ай бұрын

    Another great video, thanks

  • @melomotive14

    @melomotive14

    Ай бұрын

    Thanks

  • @SwiftRIBSAust
    @SwiftRIBSAustАй бұрын

    Excellent vid.

  • @melomotive14

    @melomotive14

    Ай бұрын

    Thanks mate

  • @lawrencehalpin6611
    @lawrencehalpin661127 күн бұрын

    Thank you Gentlemen for the terrific lesson on metal work. Kind regards.

  • @melomotive14

    @melomotive14

    10 күн бұрын

    Your welcome.

  • @wayneodonnell8847
    @wayneodonnell8847Ай бұрын

    Awesome video guys

  • @melomotive14

    @melomotive14

    Ай бұрын

    Thanks

  • @abdulhamoui4376
    @abdulhamoui437628 күн бұрын

    well explained guys!

  • @melomotive14

    @melomotive14

    27 күн бұрын

    Thanks.

  • @user-bu3ee3nu1s
    @user-bu3ee3nu1s24 күн бұрын

    Great work fellas.

  • @melomotive14

    @melomotive14

    10 күн бұрын

    Thanks

  • @undeadarkhantheblack
    @undeadarkhantheblack26 күн бұрын

    Great video, nice tricks. Thanks a lot

  • @melomotive14

    @melomotive14

    10 күн бұрын

    You're welcome!

  • @poydapoyderson646
    @poydapoyderson646Ай бұрын

    Really really handy video. I know there are heaps of scenarios. I have a Holden Ute with high and low spots right along the 'banana' body lines. Would you guys do some vids on dents on body lines, both in and out. This one you did was obviously easier as you could reach dolly under, any tips where you can't?

  • @melomotive14

    @melomotive14

    Ай бұрын

    Thanks mate. Absolutely planning on more. Dents with limited access is definitely something we need to cover.

  • @Carlosdejackyl959
    @Carlosdejackyl95922 күн бұрын

    I'm surprised nobody uses a nice soft rag between their palm and the surface to feel for highs and lows.

  • @bobmcdougal7501
    @bobmcdougal750125 күн бұрын

    Maybe not show every hammer and slapper hit in fast motion. Seeing how lightly he makes the strike would be of paramount importance. Thank God for closed captioning. 😊

  • @melomotive14

    @melomotive14

    10 күн бұрын

    Thanks, will keep it mind for the next one.

  • @hectorguerrero4608
    @hectorguerrero4608Ай бұрын

    Does Peter have a KZread channel or any other kind of social media?

  • @melomotive14

    @melomotive14

    Ай бұрын

    Yes, look up “mobile car restoration” he’s on most social platforms.

  • @SkaterStimm
    @SkaterStimm22 күн бұрын

    Please show the panel after you are done with it! How perfect can you get it with the blue dykem?

  • @melomotive14

    @melomotive14

    10 күн бұрын

    Will do, this roof will be used on a project we're planning on documenting.

  • @madmorrie1100
    @madmorrie110027 күн бұрын

    Great video guys. Curious about the dye, if sharpie can bleed through paint why not the dye? I've used a big fat sharpie on a door the same way, but now wondering if that was a bad idea.

  • @melomotive14

    @melomotive14

    27 күн бұрын

    Hi mate. Some permanent markers contain an acid, that help bind the pigment to a surface. If enough acid is left on the surface it can bleed through a coating later. If you have sanded and cleaned the steel thoroughly it should be fine. We felt it was an important fact to mention. The marking dye creates a film that sits top of the surface.

  • @SwiftRIBSAust
    @SwiftRIBSAustАй бұрын

    Can you give us a bit more info on the blue dye - is it toolmakers ink ?

  • @melomotive14

    @melomotive14

    Ай бұрын

    The one we used here is a custom mix we’re playing with. But, yes, engineers marking fluid/die is very commonly used.

  • @mrgreezy1

    @mrgreezy1

    Ай бұрын

    No it’s called “Dykem” it’s just for covering the metal surface so when you go over it with a file or a sander it shows the high and low spots in the metal surface.

  • @stevegus2845

    @stevegus2845

    29 күн бұрын

    @@mrgreezy1 Same Same

  • @uncleronny6748

    @uncleronny6748

    28 күн бұрын

    Back when I did a ton of metal finishing I used the mushroom head that comes with an electric stud puller for better heat control ( Even though I have a gas torch with an auto relighter). Also, for beginners, you will find using a light cotton glove on the hand you are feeling the metal with will amplify damage. And if you are a beginner I wouldn't recommend a 356 as your first attempt as they are very challenging hence the requisite adjustable vixen file frame.

  • @andrewference1479
    @andrewference147918 күн бұрын

    Has that blue dye been thinned out? What did you use?

  • @melomotive14

    @melomotive14

    10 күн бұрын

    Yes, it has here. We're experimenting with different formulas.

  • @michaelbyrnes7944
    @michaelbyrnes794419 күн бұрын

    Now show me that on a xd xe flat roof skin. A big old round roof is easy 😂

Келесі