What about cleaning the pipe and the coupling with alcohol wipes ?? 🤦♂️
@_1ben
Жыл бұрын
I was trained no wipes with this method, the wipes with service tees and branching saddle
@biswajitpatra47122 жыл бұрын
Nice
@_1ben Жыл бұрын
Imo met fit system is cheaper, much faster install, no cooling, and way easier, do you agree? I believe this is the only option over 2" ?
@Nickbaldeagle022 жыл бұрын
Just did this today. We just hand scraped with a scraper. Vertical lines. I suspected we weren't doing it by the book. Now I know we weren't.
@holdencommodore4546
2 жыл бұрын
Scraper is Fine all it is is to clean the surface of the PE as long as its clean, and ready for the fitting to be Electrofused .. I use a hand scraper on PE from 10mmPE up too 100mmPE
@franciskharkongor9039
9 ай бұрын
We don't have the sraper after the Welding
@franciskharkongor9039
9 ай бұрын
I min to remove the sraper
@ManishSharma-zc4vb2 жыл бұрын
What's name of equipment that you using for scraping PE pipe
Пікірлер: 15
Great technology
What about cleaning the pipe and the coupling with alcohol wipes ?? 🤦♂️
@_1ben
Жыл бұрын
I was trained no wipes with this method, the wipes with service tees and branching saddle
Nice
Imo met fit system is cheaper, much faster install, no cooling, and way easier, do you agree? I believe this is the only option over 2" ?
Just did this today. We just hand scraped with a scraper. Vertical lines. I suspected we weren't doing it by the book. Now I know we weren't.
@holdencommodore4546
2 жыл бұрын
Scraper is Fine all it is is to clean the surface of the PE as long as its clean, and ready for the fitting to be Electrofused .. I use a hand scraper on PE from 10mmPE up too 100mmPE
@franciskharkongor9039
9 ай бұрын
We don't have the sraper after the Welding
@franciskharkongor9039
9 ай бұрын
I min to remove the sraper
What's name of equipment that you using for scraping PE pipe
@connorbenzie7117
2 жыл бұрын
End prep tool/ rotary scraper
Number aap log dalo technicians ka