Casting Defects | Dental Materials | Super Simple
This video on Casting defects from Dental Materials includes defects like Porosity, Incomplete casting, distortion, and surface roughness. The casting defect topic is a very important topic for dental students and exam like MDS entrance NEET Exam, NBDE. The questions are generally on localized shrinkage porosity, Suckback porosity, Backpressure porosity. The video explains these things in a simplified way with diagrams too. Easy dentistry at Aspire32 helps grasp such topics of Dentistry in the simplest possible way for dental students and dentists. Casting defect in dentistry is a difficult topic.
This video of Aspire 32 is made by Dr. Suresh Shenvi who has cleared various exams like ADAT, NBDE from the USA, DHA from Dubai, and various Indian Entrance exams like PGI, KCET, NEET. I am MDS in Conservative Dentistry and Endodontics by profession. I am also an author of dental books on the entrance exam and I am also currently a faculty at KLE University and a receiver or best teacher award.
Click The Following Link To Subscribe To My Channel Aspire 32
kzread.info?su...
Link for Complete Playlist on Cast Restorations
• Inlay and Onlay - Cast...
Link for Complete Playlist on Fundamentals of Cavity Preparation.
• Fundamentals of Tooth ...
Link for Complete Playlist on Dental Composite
• Dental Composite
Link for Complete Playlist on Glass Ionomer Cement and its types.
• Glass Ionomer Cement (...
Link for Complete Playlist on Pulp and Periapical Diseases
• Pulp and Periapical Di...
Link for Complete Playlist on Pulp Protection ( Direct and Indirect Pulp capping)
• Pulp Protection - Varn...
Link for Complete Playlist various Dental Product reviews
• Review of Endodontics ...
#aspire32, #sureshshenvi,
Пікірлер: 64
Thank you so much sir , with clear concept help me a lot helping a lot in solving Mcqs in neet
@Aspire32
3 жыл бұрын
Glad to hear that. I am happy the channel is meeting its purpose :)
I've never would've understand this topic if i did'nt see this. You explained it so well! Thank you so much sir
@Aspire32
3 жыл бұрын
Thank you for the kind words :).. That really made my day :)
Thank you so much for this awesome series of videos on Cast restorations.. Wish I understood cast restorations so clearly during the college.. Thank you once again and God bless you!!!
@Aspire32
3 жыл бұрын
So happy to hear that you finally understood the topic better. Do check this video on prepration for cast Restoration. kzread.info/dash/bejne/dqWBw6WRfJrXoKw.html
I was struggling with this topic... Finally got my concept cleared.. Thank you so much sir😊
@Aspire32
3 жыл бұрын
This is what makes me super happy. Knowing its helping students understand better :) do subscribe to the channel Here is are few more videos related to cast Restoration kzread.info/head/PLdPsg6P-6VlcG-msLe6BvhIz9p3QYx4VY
Much needed topic. Wonderfully explained sir. ,👍👍
@Aspire32
3 жыл бұрын
Thank you Pankhuri :)
Awsome .videos....keep.uploading🙏🙏🙏👍👍👍👍👍👍👍👍👍👍👍
@Aspire32
3 жыл бұрын
Sure. There are many useful videos. Do check them :) .. Hope you will Subscribe :)
Majestically put, Full of wisdom and intellect. Love and Respect from Kashmir.
@Aspire32
2 жыл бұрын
Thank you so much dear :):)
Sir you explain soo well that everything seems so easy A heartfelt thanks to you 😊
@Aspire32
3 жыл бұрын
Thank you. I just explain the same thing which is there in textbook :) Do Check the new video just released today. Rotary Cutting instruments covers type of Handpieces, Speed, Types of burs, the various angle like Rake Clearance angle, Edge angle in a Super Simple Way ! kzread.info/dash/bejne/gKWlm7mkhZS-qJs.html
I had read it like so many times but i dint get it, now i listened to this n went to pulse to solve MCQ, i could ans then all , thank you so much sir, no words 👏👏
@Aspire32
Жыл бұрын
Absolutely. Things do not have to be so complicated isn't it ?. I am glad you found it useful
Neatly explained sir.... upload more like this ....
@Aspire32
3 жыл бұрын
Thank you Dr Ajay :)
Thank you sir..Your videos going to help a lot ..
@Aspire32
3 жыл бұрын
Welcome Vinod. Do share it with others :)
Simply amazing!!
@Aspire32
3 жыл бұрын
Thank you. Hope you will check the other videos too :)
Best video 💯🙏🏽🙏🏽 Thank you sir.
@Aspire32
2 жыл бұрын
So happy to hear that :)
Helping a lot , thanks for guidance 🙏
@Aspire32
3 жыл бұрын
Glad to hear that :). I hope you will check the other videos. Do check the dental Ceramics video if you always found that difficult too :)
Thanku soo much sir..You explained every point to the deapth
@Aspire32
2 жыл бұрын
Most welcome :):)
Thankyou sir for making DM that much easier for us 💃😃
@Aspire32
3 жыл бұрын
Most welcome. Do check the other dental Material videos here. Also do check operative videos on the channel kzread.info/head/PLdPsg6P-6VldkI_N1LglBPGc114Ksq9Ir
Nicely explained..thnks😄
@Aspire32
Жыл бұрын
So glad..do check other videos
You have a skill for teaching.
@Aspire32
Жыл бұрын
so happy to hear :)
Sir .....u and ur lectures are best....
@Aspire32
10 ай бұрын
Thanks for the appreciation
This was really helpful, thankyou!!!
@Aspire32
Жыл бұрын
Most welcome. Do visit the playlist sections. I have made many more Simplified
Sir you mentioned that localized shrinkage porosity occurs internally and to visualize that , we need to cut through the casting..... Can you please explain this?. Rest everything was crystal clear... Thank you so much
@Aspire32
Жыл бұрын
It means that it happens internally. You dont see it usually
Tq so much sir it helped me a lot.
@Aspire32
Ай бұрын
You are most welcome
❤❤
@Aspire32
3 жыл бұрын
Thank you :)
Sir, please reply When the metal shrinks on solidification, the shrinkage is towards which direction? How exactly the investment material expansion compensates for it ? Is the shrinkage towards outside? As shown at 2.45
@Aspire32
2 жыл бұрын
I did mention about it in the video
Excellent
@Aspire32
2 жыл бұрын
Thank you :):)
Sir can you please explain about class 2 modifications of cavity preparation
@Aspire32
3 жыл бұрын
Yes, The topic is in my list.. Will make it .. Hope you checked my earlier video on class 2 Link kzread.info/dash/bejne/kWxppKOTcZnKqNI.html
Sir investment Powder what's how stor purchase
Super sir☺️
@Aspire32
2 жыл бұрын
Thanks :)
🙏🙏🙏
@Aspire32
3 жыл бұрын
Thank you. Pls do check kzread.info/head/PLdPsg6P-6VlcG-msLe6BvhIz9p3QYx4VY
How to decide which investment material to use for which wax which properties should be similar
@Aspire32
Жыл бұрын
It depends on the metal alloy one will be using for casting
Sir please make a video on investment materials 🙏
@Aspire32
Жыл бұрын
I will definitely try :)
Can u explain distortion (due to investment material) ...unable to understand please?
@sidrabajwa9397
2 жыл бұрын
You mean when mould expand...can pattern also explain which leads to porosities ?
@Aspire32
2 жыл бұрын
Yes. It pulls the pattern with it