Amazing Process : Hot-Dip Galvanized U Bolts Process | How To Galvanize Bolts
in this video we see the amazing process of How To galvanized U bolt and nut bolts. #galvanized #process #bolts
Жүктеу.....
Пікірлер: 23
@INFOROYALSTEELGALVANIZER-ee2nrАй бұрын
Frm india chemical using for not splittering zinc during dipping
@gantry289 Жыл бұрын
Thanks for the video. I know it would be hard and a lot of work but sometimes I wish you could put some descriptions in the video. Things like they use recycled metal from... or in this case, they first put the u bolts in a acid bath to clean them and remove any rust or oils, They heat the zinc ingots to ?C degrees etc. Wonder why they have that pile of dirt onto on the smelter? It seemed like some of it kept getting into the zinc bath
@atomthings7923
Жыл бұрын
Thanx for the suggestion next time I’ll put some description about process ✌️
@lakhrajmahour3187
9 ай бұрын
YOUR MOBIL NO @@atomthings7923
@damnwereinatightspot
3 ай бұрын
@@atomthings7923 thank you ill look for some. Amazing process
@JoeLintang7 ай бұрын
what chemical solution to use for soaking ? thanks
@jinsonrajan22
Ай бұрын
@JoeLintang it is acid either Hydrochloric Acid or Sulphuric acid for removing mill scales and rust
@JoeLintang
Ай бұрын
@@jinsonrajan22 thanks
@dodi39117 ай бұрын
Untul pembakaran apakah menggunakan kayu bakar?
@binoyadhikary12817 ай бұрын
Vai ap kaha se ho
@ZIGUITAI7 ай бұрын
good video ,what size is the zinc bath ?
@atomthings7923
7 ай бұрын
No idea
@aminkingkhan83345 ай бұрын
Where is this place?
@atomthings7923
3 ай бұрын
its in Pakistan
@ayaanmughalofficial56949 ай бұрын
Contact person Shafiq ahmed from Nooh Engineering Works
@aminkingkhan83345 ай бұрын
Location plz
@atomthings7923
5 ай бұрын
Lahore Pakistan
@aminkingkhan8334
5 ай бұрын
@@atomthings7923 bro ap ka number mil sakta ha or Lahore ma kon si location par ha
@ShilpaM-sb1qh8 ай бұрын
Need to know more about the process please share contact details 🙏
@flamianjabz5 ай бұрын
Any contact information? Like addres or phone number?
Пікірлер: 23
Frm india chemical using for not splittering zinc during dipping
Thanks for the video. I know it would be hard and a lot of work but sometimes I wish you could put some descriptions in the video. Things like they use recycled metal from... or in this case, they first put the u bolts in a acid bath to clean them and remove any rust or oils, They heat the zinc ingots to ?C degrees etc. Wonder why they have that pile of dirt onto on the smelter? It seemed like some of it kept getting into the zinc bath
@atomthings7923
Жыл бұрын
Thanx for the suggestion next time I’ll put some description about process ✌️
@lakhrajmahour3187
9 ай бұрын
YOUR MOBIL NO @@atomthings7923
@damnwereinatightspot
3 ай бұрын
@@atomthings7923 thank you ill look for some. Amazing process
what chemical solution to use for soaking ? thanks
@jinsonrajan22
Ай бұрын
@JoeLintang it is acid either Hydrochloric Acid or Sulphuric acid for removing mill scales and rust
@JoeLintang
Ай бұрын
@@jinsonrajan22 thanks
Untul pembakaran apakah menggunakan kayu bakar?
Vai ap kaha se ho
good video ,what size is the zinc bath ?
@atomthings7923
7 ай бұрын
No idea
Where is this place?
@atomthings7923
3 ай бұрын
its in Pakistan
Contact person Shafiq ahmed from Nooh Engineering Works
Location plz
@atomthings7923
5 ай бұрын
Lahore Pakistan
@aminkingkhan8334
5 ай бұрын
@@atomthings7923 bro ap ka number mil sakta ha or Lahore ma kon si location par ha
Need to know more about the process please share contact details 🙏
Any contact information? Like addres or phone number?